WebMar 17, 2016 · Microstructure, phase composition and mechanical properties of a refractory high entropy superalloy, AlMo0.5NbTa0.5TiZr, are reported in this work. The alloy consists … WebThere has been also recent interest in exploring the possibility of so-called refractory high-entropy superalloys (RSAs). These are also multicomponent refractory alloys featuring, however, dual-phase microstructures with disordered bcc A2 and ordered B2 phases, which could result in improved mechanical properties.
B2 ordering in body-centered-cubic AlNbTiV refractory high …
WebOct 12, 2024 · The recently developed refractory metal high entropy superalloys (RSA) have been proposed as novel materials for high temperature service. A key requirement of any material used in such... WebAug 8, 2024 · Controlled Al-induced B2 ordering helps overcome the strength-ductility dilemma in refractory medium-entropy alloys due to solid solution and short-range strengthening coupled with the dislocation motion changing. KEYWORDS: Refractory medium-entropy alloys B2 ordering short-range order strength-ductility trade-off … cross stitch shops in georgia
Development of a Refractory High Entropy Superalloy
WebMar 17, 2016 · Microstructure, phase composition and mechanical properties of a refractory high entropy superalloy, AlMo 0.5 NbTa 0.5 TiZr, are reported in this work. The alloy consists of a nano-scale mixture of two phases produced by the decomposition from a high temperature body-centered cubic (BCC) phase. WebJun 10, 2024 · Refractory high-entropy alloys (RHEAs) have garnered a lot of attention over the past decade for their potential for high-temperature structural applications (Senkov et al., Reference Senkov, Wilks, ... Refractory high entropy … WebRefractory high entropy superalloys (RSAs) Daniel B. Miracle, Ming Hung Tsai and 3 more Open Access October 2024 Volume 187, Pages 445-452 Machine learned feature identification for predicting phase and Young's modulus of low-, medium- … build a life size r2d2